HMLS polyester yarn
TEST PARAMETERS | UNIT | 1000D/304F (1100dtex) | 1300D/320F (1440dtex) | 1500D/376F (1670dtex) | 2000D/564F (2200dtex) |
GRADE | A | A | A | A | |
LINEAR DENSITY | dtex | 1120±30 | 1450±30 | 1680±30 | 2230±30 |
BREAKING STRENGTH | N(min) | 76 | 99 | 115 | 152 |
ELONGATION AT BREAK | % | 12.0±2.0 | 12.0±2.0 | 12.0±2.0 | 12.0±2.0 |
H.A.S. AT 177℃,1MINS | % | 3.5±0.8 | 3.5±0.8 | 3.5±0.8 | 3.5±0.8 |
ELONGATION AT SPECIFIC LOAD 4.0CN/dtex | % | 5.5±0.8 | 5.5±0.8 | 5.5±0.8 | 5.5±0.8 |
OIL CONTENT | % | 0.5±0.2 | 0.5±0.2 | 0.5±0.2 | 0.5±0.2 |